PROFIS ENGINEERING REPORT SHEAR LOAD

Concrete Breakout Failure Mode
Results ϕ nonductile
Results 318-14 Chapter 17 Provision Comments for PROFIS Engineering
ϕ nonductile
ACI 318-14 Section 17.2.3.4.4
17.2.3.4.4 The anchor design tensile strength for resisting earthquake forces shall be determined from consideration of ( a ) through ( e ) for the failure modes given in Table 17.3.1.1 assuming the concrete is cracked unless it can be demonstrated that the concrete remains uncracked :
( a ) ϕN sa for a single anchor or for the most highly stressed individual anchor in a group of anchors ( b ) 0.75ϕN cb or 0.75ϕN cbg except that N cb or N cbg need not be calculated where anchor reinforcement satisfying 17.4.2.9 is provided ( c ) 0.75ϕN pn for a single anchor or for the most highly stressed individual anchor In a group of anchors ( d ) 0.75ϕN sb or 0.75ϕN sbg
( e ) 0.75ϕN a or 0.75ϕN ag where ϕ is in accordance with 17.3.3 .
ACI 318-08 Part D . 3.3.6
D . 3.3.6 — As an alternative to D . 3.3.4 and D . 3.3.5 , it shall be permitted to take the design strength of the anchors as 0.4 times the design strength determined in accordance with D . 3.3.3 . For the anchors of stud bearing walls , it shall be permitted to take the design strength of the anchors as 0.5 times the design strength determined in accordance with D . 3.3.3 .
When designing an anchorage for seismic tension load conditions , ACI 318-14 provisions for concrete breakout failure in tension require calculation of a nominal concrete breakout strength ( N cb or N cbg
). The nominal strength is multiplied by two strength reduction factors ( ϕ-factors ): one ϕ
-factor for concrete breakout failure in tension , and one ϕ
-factor for seismic tension load conditions , to obtain a design strength ( 0.75ϕN cb or 0.75ϕN cbg
).
PROFIS Engineering designates the 0.75 seismic tension reduction factor noted in ACI 318-14 Section 17.2.3.4.4 “ ϕ seismic
”. This reduction is only considered with respect to non-steel tension failure modes when calculating tension design strengths for both cast-in-place and post-installed anchors subjected to seismic tension loads .
When designing an anchorage for seismic shear load conditions , ACI 318- 14 strength design provisions for concrete breakout failure in shear require calculation of a nominal concrete breakout strength ( V cb or V cbg
) that is only multiplied by one ϕ-factor to obtain a shear design strength ( ϕV cb or ϕV cbg ).
PROFIS Engineering designates this ϕ-factor “ ϕ concrete ”. The 0.75 seismic strength reduction factor ( ϕ seismic
) required per Section 17.2.3.4.4 is only relevant to tension calculations , and is therefore not applied to V cb or V cbg when the anchorage is being designed for seismic shear load conditions . The parameter “ ϕ nonductile
” is a reduction factor for seismic tension and seismic shear load conditions that is given in Part D . 3.3.6 of the anchoring-to-concrete provisions in ACI 318-08 Appendix D . This reduction factor can range from a value of 0.4 to 1.0 , depending on the application , and PROFIS Engineering designates this factor “ ϕ nonductile
”.
“ ϕ nonductile
” is not a relevant parameter for seismic design per ACI 318-14 Chapter 17 ; therefore , it is always referenced in the PROFIS Engineering report for ACI 318- 14 calculations as equal to 1.0 .
Reference the PROFIS Engineering Design Guide for ACI 318-08 anchoring-toconcrete provisions for more information on ϕ nonductile
.
202 NORTH AMERICAN PROFIS ENGINEERING ANCHORING TO CONCRETE DESIGN GUIDE — ACI 318-14 Provisions