Fig
. 3. a) Digital holographic image of GUW on the surface of an aluminum sample of 32.0 cm 9.4 cm 2.6 cm resulting from a piezo excitation with f Exc = 200 kHz. b) By statistical analysis of the measured height distribution with the SF, the wavelength of the GUW is given by the position of the first local minimum at s 0 = 10.7 ± 0.8 mm. Overall, the multidirectional SF makes a periodicity visible, despite the superposition of various waves on the surface.
Fig
. 4. a) GUWs on aluminum plates with different thickness d 1 = 2.6 mm( red) and d 2 = 5.0 mm( black) are excited at different frequencies f Exc = [ 60, 300 ] kHz in steps of 20 kHz. By means of digital holography, the surface deformation is then measured and evaluated with the structure function to determine the wavelength k m of the GUW, which is plotted against f Excd. The thinner plate shows shorter wavelengths. b) The measured wavelengths are plotted against the resulting wavelengths from the simulation for the A0 mode k sim. The blue line marks the ideal result for the case of k m = k sim, corresponding to a slope of m = 1. The experimental results are in agreement with the simulation results for both samples. The corresponding slopes are m 1 = 0.95 and m 2 = 1.08. This successfully qualifies our measurement method for the measurement and characterization for GUWs.
simulation, only the wavelength k sim of the fundamental antisymmetric mode is used as a function of the frequency f Exc. The reason for this is that the fundamental antisymmetric mode has the highest out-of-plane displacement in the investigated frequency range.
3 Results for aluminum plates with different thickness
After the subsequent recording of the two holograms, the holograms were spectrally filtered and numerically reconstructed using the Fresnel approximation, resulting in a pixel pitch of Dn =( 52 ± 4) lm in the reconstructed image. Then, the phase difference was calculated and translated into height values. In Figure 2 some exemplary height distributions can be seen, featuring visible periodic deformations on the surfaces of sample 1 and 2 at different excitation frequencies f Exc.
In Figure 3a, we see another example for a digital holographic measurement of the deformation on sample 1 caused by GUWs at f Exc = 200 kHz. Due to the superposition of different waves, caused by the continuous excitation and reflections from the edges, there is no clear propagation direction of the GUWs. Nevertheless, a periodicity can be seen. To characterize the GUWs, the structure function is then applied to the whole surface. As seen in Figure 3b, the periodicity is reproduced with the SF. In this case, the measured wavelength k m is determined to k m = 10.7 ± 0.8 mm from the position of the first local minimum. For this statistical analysis, all surface points are taken into account.