Figure 3. Laser performances at 3500 nm for 70 % output coupling ratio:( a) Laser power stability over 5 h for 1 W output power.( b) M 2 measurements of the output laser beam.
Figure
4. PER measurements as a function of wavelength in the case of T OC = 30 %( a) and T OC = 70 %( b). Insets: Typical linear polarization measurement results with theoretical fit( Malus’ law) for laser emission at 3414 nm with T OC = 30 %( a) and for laser emission at 3500 nm with T OC = 70 %( b).
After a slight initial decrease due to thermal stabilization, the power remained stable throughout the experiment with an overall rms deviation of 0.81 %. The M 2 measurement was performed using a 200 mm focal length CaF 2 lens and our Pyrocam. Figure 3b shows the results which highlight the excellent beam quality, with an M 2 of 1.09( resp. 1.05) on the x-axis( resp. y-axis). This slight astigmatism is most likely due to the PM operation of the fiber. The air holes surrounding the core deconfine the mode on one axis, resulting in a slightly elliptical mode.
3.3 Output power scaling
Figure 2c shows the evolutions of the output powers at key wavelength points with respect to the launched pump power at 1975 nm for fixed 976 nm pump power. Increasing the 976 nm pump power allows to supply sufficient population on the 4 I 11 / 2 and thus more gain for lasing at long wavelengths. The pumping power at this wavelength is relatively low compared to the pumping needed for low doped Erbium fluoride fibers as they exhibit rapid quenching effects when increasing the 1975 nm pump power [ 19, 20 ]. At the central wavelength of 3500 nm, a maximum output power of 1.61 W of polarized laser light was achieved for a pump power of 20 W at 1975 nm, which corresponds to an
efficiency of 11 %( with respect to the 1975 nm pump power). We note that the calculated slope efficiency with respect to the 1975 nm pump power injected into the fiber is about 14 %. This watt-level power was achieved for the whole range of 3400 – 3600 nm although with varying efficiencies. Beyond this wavelength range, high output powers were also achieved, for instance at 3670 nm with 830 mW, which corresponds to an efficiency of 6.7 %. Note that even if heavily doped Erbium fluoride fibers do not exhibit rapid quenching effects, the heavy doping induces rapid heating compared to low doped fibers. This effect combined with the high thermal expansion coefficient of fluoride glass( 20010 �7 K �1) putsthefiber facets at risk of damage limiting further power scaling. This also induces a mechanical“ shift” of the fiber core making it necessary to adjust the injection of the 1975 nm pump when increasing the pump power. This explains the small fluctuations that can be seen on the experimental measurements when increasing the 1975 nm pump power. For pump powers higher than 21 W, strong output power fluctuations are observed which is usually an indication that the fiber facet is starting to get damaged. To avoid any fiber damage, we explored the pump power range below 21 W where the laser exhibited an excellent output power stability over the whole wavelength range.